Product Description

Product overview
2055 thermal phase change materials based on synthetic paraffin base material, join the high-performance thermal conductive particles.Convenient and cutting into various shapes, stick in the cooling area;After the phase transition can be filled with tiny gap.Products both thermal conductive paste (liquid) low thermal resistance characteristics of level, and having the features of ordinary piece of easy to operation of thermal conductivity, thermal paste is natural alternatives, save the cumbersome process of screen printing, small size is easy to store.


Product features
1. The flake, easy to use.
2. The thermal resistance is low, one-time full of cracks after phase transformation
3. Long life and stability
4. Interstitial skills (phase change expansion rate is about 15%)


Color appearance
Gray visual
The thickness of mm
0.1 0.5 Brookfield DV - 3
G/cm3 density
1. 3 g
2.8 ASTM D374
Coefficient of thermal conductivity W/m.k
The thermal resistance of 20 psi
80 psi ℃. W/in2
6-8 w ASTM D5470
0.06
0.08 ASTM D5470 Modify




Volume resistivity Ω · cm
2 * 1014 GB/T 1410
Shaw hardness Share A
< 80 ASTM D2240
The electric strength KV/mm
0.46 ASTM D149
Working temperature
- 40-150 ℃ for a long time
Phase change temperature ℃
45 E794
Storage temperature ℃
10-23 -